Jewellery Trouble Shooting Wax Pattern Problems

Mould over fills

REMEDY : Reduce air pressure
REMEDY : Adjust temperature
REMEDY : Held plates firmly,distributing pressure evenly over

REMEDY :
Entire mould surface.

REMEDY :
Hold for less time.

Mould not filling

REMEDY :
Adjust air pressure.

REMEDY :
Adjust temperature.

REMEDY : Remove and clean.
REMEDY : Hold without squeezing.
REMEDY : Clean plates so surfaces are flat.
REMEDY : Make air release cuts(vents) in mould. Be sure wax pot is more than ½ full.
REMEDY : Warm mould

Air bubbles in pattern

REMEDY : Adjust air pressure
REMEDY : Add wax. Be sure that wax pot is more Than ½ full.
REMEDY : Adjust temperature and stir wax to release trapped air.

REMEDY : Held muold on same plane as nozzle.

Wax brittle

REMEDY : Check temperature of platens.
REMEDY : Use new wax. Use no less than 90% new wax with reused. Try avoiding using old wax.
REMEDY : inject fewer moulds during production cycle.
REMEDY : Use wax that is suitable to type of pattern beingproduced.

Wax discoloured (brownish)

REMEDY : Clean wax pot (steam or soak in Percloroethylene);add new wax.

Pattern bend easily, wax sticks to mould

REMEDY :  Adjust temperature.

REMEDY : Prolong cooling period by working more moulds.

Wax keeps flowing after mould is filled

REMEDY : Remove and clean nozzle.